Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.33 GPa | 1643 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 11.33 GPa | 1643 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RX00713H PA 66 LNP* Thermocomp* RX00713H is a compound based on Nylon 6/6 containing proprietary fillers. Characteristics of this grade are: Healthcare. |