Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0780 GPa | 11.3 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 8502-SR BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.0779 GPa | 11.3 ksi | 1% Sec; ASTM D-790-92 |
Multibase Multi-Flex® TPE A 8592 MEDIUM TAUPE Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Krato.. |
|||
Flexural Modulus | 0.0780 GPa | 11.3 ksi | ASTM D790 |
Arkema Group Pebax® MX 1205 Polyether Block Amide (PEBA) Typical application: Impact modifierInformation provided by Arkema Group |