Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.30 - 7.50 GPa | 334 - 1090 ksi | Average value: 5.04 GPa Grade Count:7 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |