Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.338 GPa | 1064 ksi | UNI EN ISO 14125: 2000 |
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its.. |