Polymer Property : Flexural Modulus = 10.965 GPa
Polymer Property :
Flexural Modulus =
10.965 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
10.965
GPa
1590.4
ksi
ASTM D790
NYCOA 27/440KNF Glass Filled Nylon 6
44% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc.