Mechanical Properties Metric English Comments
Flexural Modulus 10.57 GPa
1533 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Verton RV008ESV PA 66
40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region.