Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.23 GPa | 1484 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan.. |