Flexural Modulus 10.21 GPa
1481 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA
LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 10.21 GPa
1481 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA (Asia Pacific)
LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized.