Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.09 GPa | 1463 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
Flexural Modulus | 10.09 GPa | 1463 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
Flexural Modulus | 10.09 GPa | 1463 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC (Asia Pacific) LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |