Polymer Property : Flexural Modulus = 1.903 GPa
Polymer Property :
Flexural Modulus =
1.903 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
1.903
GPa
276.0
ksi
ASTM D790
NYCOA 2047 Copolymer Nylon 6/69
extrusion, high melt viscosity. & strength., low crystallinity Information provided by NYCOA, Inc.