Mechanical Properties Metric English Comments
Flexural Modulus 1.8264 GPa
264.89 ksi
ASTM D790
BCC Products BC 8405 Urethane Casting
BC8405 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8405 will exhibit high impact strength and yield thermoplastic-like parts. Some features i..