Mechanical Properties Metric English Comments
Flexural Modulus 1.765 GPa
256.0 ksi
ASTM D790
Tipco Tipcolene® FPC 10 - 10% Calcium Carbonate Reinforced Polypropylene Homopolymer
10% Calcium Carbonate Filled PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Modulus 1.765 GPa

@Temperature 260 °C
256.0 ksi

@Temperature 500 °F
ASTM D790
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca..