Mechanical Properties Metric English Comments
Flexural Modulus 1.759 GPa
255.1 ksi
1% Secant; ASTM D 790
Chevron Phillips HiD® 9706 HDPE Injection Molding Resin  (discontinued **)
Resin Type: linear homopolymerCharacteristics: moderate flow, good impact strength, excellent stiffness, good ESCR, moderate shrinkage resistanceApplications: crates and totes, structural foamInform..
Flexural Modulus 1.759 GPa
255.1 ksi
tangent; ASTM D790
Entec Hypro™ PPC-T20 Copolymer Polypropylene, 20% Talc Reinforced
Information provided by Entec