Polymer Property : Flexural Modulus = 1.585 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.585 GPa
229.9 ksi
ASTM D790
Eastman Tritan EX401 Copolyester
Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are..
Flexural Modulus 1.585 GPa
229.9 ksi
ASTM D790
Eastman Tritan LX201 Copolyester
Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are..
Flexural Modulus 1.585 GPa
229.9 ksi
ASTM D790
Eastman Tritan MX810 Copolyester
Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re..
Flexural Modulus 1.585 GPa
229.9 ksi
ASTM D790
Eastman Tritan MX811 Copolyester
Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceGood heat resistanceO..
Flexural Modulus 1.585 GPa
229.9 ksi
ASTM D790
Eastman Tritan TX2000 Copolyester
Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc..
Flexural Modulus 1.585 GPa
229.9 ksi
ASTM D790
Eastman Tritan TX2001 Copolyester
Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe..
Flexural Modulus 1.585 GPa
229.9 ksi
tangent; chs 0.05 in/min; ASTM D790
Diamond Polymers Centrex® 601 Profile Extrusion Grade AES
Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can..
Flexural Modulus 1.585 GPa
229.9 ksi
chs 0.05 in/min; 1% secant; ASTM D790
Diamond Polymers NPP30-1200S Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 1.585 GPa
229.9 ksi
ISO 178
Cathay PA511 Renewable Engineering Polyamide
Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr..