Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.500 GPa | 217.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C10L Calcium Reinforced |
|||
Flexural Modulus | 1.500 GPa | 217.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336W10L1 Wollastonite Reinforced |
|||
Flexural Modulus | 1.500 GPa | 217.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339C10L1 Calcium Reinforced |
|||
Flexural Modulus | 1.500 GPa | 217.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436T20L Talc Reinforced |
|||
Flexural Modulus | 1.500 GPa | 217.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene CP0405UVV Copolymer UV Stabilized Approved to Suzuki PP-S2 Med Grey T01 |
|||
Flexural Modulus | 1.500 GPa | 217.5 ksi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N2300STHL BK Post Consumer Recycle Nylon 6 Superior Toughness, Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |