Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.310 GPa | 190.0 ksi | ASTM D790 |
Lucent Polymers CPP-210 Polypropylene, 10% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |