Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.205 GPa | 174.8 ksi | Tangent-Method 1; ASTM D790 |
Ineos G50-100 HDPE Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding p.. |