Mechanical Properties Metric English Comments
Flexural Modulus 1.151 GPa
166.9 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 150-1501 HDPE Rotational Molding Resin
Description: ICORENE 150-1501 is a high density polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability..