Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1.09 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.09 GPa
158 ksi
Chord; 2 mm/min; ISO 178
Mytex Polymers AS43L-01 Polypropylene, Rubber modified, Compounded
Description: AS43L-01 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key..
Flexural Modulus 1.09 GPa
158 ksi
2% secant; ASTM D790-02
Ipiranga Petrochem HA 7260 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Flexural Modulus 1.09 GPa
158 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU
LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity.
Flexural Modulus 1.09 GPa
158 ksi
ASTM D790
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..
Flexural Modulus 1.09 GPa
158 ksi
Secant, 0.079 in/min; ISO 178
ExxonMobil Exxtral™ H1025W Performance Polyolefin
Product Description: A polyolefin injection molding compound designed with good flow, cold temperature impact resistance, low CLTE, weatherable mold-in-color and also suitable for painted automotive..
Flexural Modulus 1.09 GPa
158 ksi
ASTM D790
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..
Flexural Modulus 1.09 GPa
158 ksi
ASTM D790
Clariant Renol PPSP0004 Polypropylene, Random Copolymer
Data provided by Clariant Masterbatches
Flexural Modulus 1.09 GPa
158 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow UNIVAL™ DMDF-6200 NT 7 High Density Polyethylene Resin (HDPE)
Excellent extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDF-6200 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipme..
Flexural Modulus 1.09 GPa
158 ksi
ASTM D-790
Bapolene® 3039U Polyethylene, Rotational Molding Grade
Bapolene 3039U is a hexene linear low density polyethylene designed to provide superior impact resistance. It contains a UV-stabilization package and complies with US FDA 21CFR177.1520.Applications..