Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.071 GPa | 155.4 ksi | 2% Secant; 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case.. |