Mechanical Properties Metric English Comments
Flexural Modulus 1.063 GPa
154.2 ksi
BCC Products MB 2001 Urethane Foam Modeling Board
MB2001 is a general purpose light weight urethane board engineered specifically to meet the tooling requirements of a wide range of applications for the automotive/aerospace, prototype, foundry, and..