Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.975 GPa | 141 ksi | ASTM D790 |
Carmel Olefins CAPILENE® TG 50 Polypropylene Impact Copolymer Description: CAPILENE® TG 50 is a heterophasic copolymer designed for injection molding applications requiring optimal impact resistance. This grade combines excellent impact strength, even at lo.. |