Mechanical Properties Metric English Comments
Flexural Modulus 0.958 GPa
139 ksi
ASTM D790
Entec Hypel® PEHD8/.955 HDPE  (discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..