Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00641 GPa | 0.930 ksi | 13 mm/min; ASTM D790 |
PolyOne FireCon™ CPE 30-33 RoHS BLACK Polyethylene, Chlorinated (CPE) An excellent choice for low-voltage power-and-cable control cables, this RoHS compliant, flexible, black colored thermoplastic CPE jacketing compound offers wire and cable manufacturers the advantag.. |
|||
Flexural Modulus | 0.00641 GPa | 0.930 ksi | 13 mm/min; ASTM D790 |
PolyOne FireCon™ CPE 32-33 RoHS Black Polyethylene, Chlorinated (CPE) An excellent choice for low-voltage power-and-cable control cables, this RoHS compliant, flexible, black colored thermoplastic CPE jacketing compound offers wire and cable manufacturers the advantag.. |