Mechanical Properties Metric English Comments
Flexural Modulus 0.892 GPa
129 ksi
ASTM D790
Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin  (discontinued **)
MR4086 is a UV stabilized, pelleted medium density polyethylene for rotomolding.Applications: Large industrial tanks, agriculture tanks, chemical drums, bins, cones, bottle caps.Advantages: Excelle..