Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.86798 GPa | 125.89 ksi | ASTM D790 |
ICO Polymers ICORENEâ„¢ 150-1496 HDPE Rotational Molding Resin Description: ICORENE 150-1496 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is.. |
|||
Flexural Modulus | 0.86798 GPa | 125.89 ksi | ASTM D790 |
ICO Polymers ICORENEâ„¢ 150-1499 HDPE Rotational Molding Resin Description: ICORENE 150-1499 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is .. |