Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.841 GPa | 122 ksi | Tangent; ASTM D790 |
Multibase Nylex™ 1230 Natural Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |
|||
Flexural Modulus | 0.841 GPa | 122 ksi | 2% Secant-Method 1; ASTM D790 |
Ineos K44-11-128 HDPE Ineos K44-11-128 is a high molecular weight, high density polyethylene copolymer intended for large part blow molding where the finished product demands good physical performance and low color. Thi.. |