Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.74994 GPa | 108.77 ksi | ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1037 LMDPE Rotational Molding Resin Description: ICORENE 115-1037 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Flexural Modulus | 0.74994 GPa | 108.77 ksi | ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1651 LMDPE Rotational Molding Resin Description: ICORENE 115-1651 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Flexural Modulus | 0.74994 GPa | 108.77 ksi | ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1654 LMDPE Rotational Molding Resin Description: ICORENE 115-1654 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |