Polymer Property : Flexural Modulus = 0.68966 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.68966 GPa
100.03 ksi
ASTM D790
Lucent Polymers PPC-320 Polypropylene, Impact Modified
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 0.68966 GPa
100.03 ksi
ASTM D790
Lucent Polymers PPC-310 Polypropylene, Impact Modified
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.