Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.608 GPa | 88.2 ksi | |
Kuraray HYBRAR® PP1 Thermoplastic Rubber-Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Flexural Modulus | 0.608 GPa | 88.2 ksi | ASTM D790 |
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5700 is an extrusion grade.Information provided by Samyang. |