Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.578 GPa | 83.8 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE D 5302 NAT The moisture content is 0.912%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |