Polymer Property : Flexural Modulus = 0.520 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.320 - 0.520 GPa
46.4 - 75.4 ksi
ASTM D790
Zeus THV Tubing
THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity.