Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.438 GPa | 63.5 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE D 5303 BLK Ash is 2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.438 GPa | 63.5 ksi | |
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2503.10 Polyethylene resin is a narrow molecular weight distribution copolymer designed as a superior processing resin. For very thin wall higher cavitation molding, this grade often is a p.. |