Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.386 GPa | 56.0 ksi | ASTM D790 |
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Blow Molding Applications) ApplicationsPETROTHENE NA 324-009 is a low density homopolymer resin intended for blow molding applications. NA 324-009 provides good clarity, toughness and processability. Typical applications in.. |
|||
Flexural Modulus | 0.386 GPa | 56.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-355 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Flexural Modulus | 0.386 GPa | 56.0 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7144 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as large industrial containers and trash cans. Information provide.. |
|||
Flexural Modulus | 0.386 GPa | 56.0 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8320 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Flexural Modulus | 0.386 GPa | 56.0 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow GRSN-9820 NT 7 Linear Low Density Polyethylene Granular Solid DOW GRSN-9820 NT 7 is produced using UNIPOL™ PE process technology and is supplied in granular form. This resin is specifically designed as a carrier resin for color concentrates and other master .. |