Polymer Property : Flexural Modulus = 0.261 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.261 GPa
37.9 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE D 4308 BLK
The moisture content is 0.04%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.