Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.260 GPa | 37.7 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP YP003 POLYESTER ELASTOMER LNP LUBRICOMP* YP003 is a compound based on Polyester Elastomer resin containing 15% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 0.260 GPa | 37.7 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas .. |
|||
Flexural Modulus | 0.260 GPa | 37.7 ksi | ASTM D790 |
Samyang Triel® 5600 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5600 is an extrusion grade.Information provided by Samyang. |
|||
Flexural Modulus | 0.260 GPa | 37.7 ksi | ASTM D790 |
Teknor Apex Telcar® TL-1477B AUTO UV BLACK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Flexural Modulus | 0.260 GPa | 37.7 ksi | ASTM D790 |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Flexural Modulus | 0.260 GPa @Temperature 120 °C |
37.7 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8253 HS PA6 (Dry) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
Flexural Modulus | 0.260 GPa @Temperature 120 °C |
37.7 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Flexural Modulus | 0.260 GPa @Temperature 120 °C |
37.7 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8270 HS PA6 (Dry) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Flexural Modulus | 0.260 - 3.90 GPa @Temperature -40.0 - 121 °C |
37.7 - 566 ksi @Temperature -40.0 - 250 °F |
Average value: 1.29 GPa Grade Count:14 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |