Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.2575 GPa | 37.35 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 6100 Injection Molding Resin
(discontinued **) LL 6100 is a narrow molecular weight butene copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications .. |