Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.213 - 0.255 GPa | 30.9 - 37.0 ksi | Secant 1%; ASTM D-790-95 |
Multibase Multi-Flex® TPO 1047-4107 Passed impact resistance 3.4J at -30°C; ASTM GM 9032 P. This product is UV stabilized for automotive applications, like fender guards and airbags.Data provided by Multibase. |