Mechanical Properties Metric English Comments
Flexural Modulus 0.240 GPa
34.8 ksi
Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790
Phillips Sumika Marlex® CHP-035 Thermoplastic Polyolefin  (discontinued **)
Applications: Painted air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.
Flexural Modulus 0.240 GPa
34.8 ksi
Shandong Guangyin PA 1212 Nylon Resin
Features and Applications: Wear resistance, higher strength, better tenacity, strong adhesion and better low temperature resistance. It is applicable to surface coating of wires, cables, optical cab..
Flexural Modulus 0.240 GPa
34.8 ksi
At 2 mm/min; ISO 178
Borealis Bormed™ LE6601-PH LDPE for Pharmaceutical Blow Molding
Bormed LE6601-PH is a LD-polyethylene produced in a high-pressure process intended for blow molding of soft and flexible packages for pharmaceutical products.Bormed LE6601-PH can be used in "blow-fi..
Flexural Modulus 0.240 GPa
34.8 ksi
ISO 178
Chengdu Polyster H6555 Thermoplastic Polyether-ester Elastomer (TPEE)
Medium modulus molding and extrusion grade. Contains improved color- stable antioxidants. Good balance of modulus and toughness. Parts and components of automobile, hydraulic hose and slide of eleva..
Flexural Modulus 0.240 GPa

@Temperature 93.0 °C
34.8 ksi

@Temperature 199 °F
ASTM Test
BASF Ultramid® 8281 HS PA6 (Dry)
Flexural Modulus 0.240 GPa
34.8 ksi
ASTM D790
Elastomer Engineering Elastamide 400 Elastomer Modified RIM Nylon 6
18% crystallinity. Information supplied by Elastomer Engineering.
Flexural Modulus 0.240 GPa
34.8 ksi
Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790
Phillips Sumika Marlex® ABF-035 Thermoplastic Polyolefin  (discontinued **)
Applications: Vehicle front-end air damsHigh impact exterior trimInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This produc..