Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.231 GPa | 33.5 ksi | ASTM D790 |
Teknor Apex Telcar® TL EF-6155 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Flexural Modulus | 0.231 GPa | 33.5 ksi | ASTM D790 |
Teknor Apex Telcar® TL EF-6155 UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Flexural Modulus | 0.231 GPa | 33.5 ksi | ASTM D790 |
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low temperature impactAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |