Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.225 GPa @Temperature 120 °C |
32.6 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8281 HS PA6 (Dry) |