Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.218 GPa | 31.6 ksi | ASTM D790 |
ExxonMobil Escorene® LL-5002 LLDPE Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. LL-5002 also exhibits good toughness and envi.. |