Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.166 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.166 GPa
24.1 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips Marlex® 1007 Injection Molding Resin
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 25200Characteristics: Excellent Flexibility, Good Flow, Good Warping Resistance, Moderate Mold Release, Good ESCRApplications:Houseware..
Copyright © lookpolymers.com All Rights Reserved