Mechanical Properties Metric English Comments
Flexural Modulus 0.0672 GPa
9.75 ksi
1% Sec; ASTM D-790-92
Multibase Multi-Flex® TPE A 8502 CLASSY GREY
Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 15%. Multi-Flex TPE contains Krato..