Polymer Property : Flexural Modulus = 0.0660 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0660 GPa
9.57 ksi
ISO 178
Chengdu Polyster FH2040 Thermoplastic Polyether-ester Elastomer (TPEE)
Blend of H2040 and self-made flame retardant material. Excellent flex resistance at low temperatures. Excellent flex-fatigue resistance. Applications requiring flexibility at low temperatures and fl..