Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0640 GPa | 9.28 ksi | ISO 178 |
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers |