Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0441 GPa | 6.40 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® A 7727 TLC Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Flexural Modulus | 0.0441 GPa | 6.40 ksi | ASTM D790 |
Multibase Multi-Flex® A 7727 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |