Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0407 GPa | 5.91 ksi | ASTM D790 |
DSM Biomedical CarboSil® 20 90A Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU) A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes Th.. |