Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.013000 GPa | 1.8855 ksi | ASTM D790 |
Sekisui PIOCELAN TOPF-30DB Flame Retardant Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |