Flexural Modulus 0.00220 GPa
0.319 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 8802 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.00220 GPa
0.319 ksi
BS4370, part 4, method 14
Zotefoams Plastazote® HL34 Polyethylene Foam